Journal of Endodontics RSS feed: Current Issue. The Journal of Endodontics , the official journal of the American Association of Endodontists , publishes scientific articles, case reports and comparison studies evaluating materials and methods of pulp conservation and endodontic treatment. Endodontists and general dentists can learn about new concepts in root canal treatment and the latest advances in techniques and instrumentation in the one journal that helps them keep pace with

Bleaching Agents Increase Metalloproteinases-mediated Collagen Degradation in Dentin

Abstract: Introduction: Tooth bleaching is based on hydrogen peroxide application. The Objective of this study was to determine whether dental bleaching agents affect metalloproteinases-mediated dentin collagen degradation.Methods: Human dentin specimens were subjected to different treatments: (1) untreated dentin; (2) demineralization by 37% phosphoric acid (PA); (3) demineralization by 37% PA, followed by application of Single Bond (SB); (4) 2 immersions of 7 days each in a nonvital bleaching agent, followed by PA; (5) 2 immersions of 7 days each in nonvital bleaching, followed by PA and SB application; (6) 3 immersions by using in-office bleaching gel for 20 minutes; (7) 3 immersions by using in-office bleaching gel for 20 minutes plus activation with a light source; and (8) immersion in home bleaching gel for 8 hours per day during 3 weeks. Specimens were stored in artificial saliva. C-terminal telopeptide determinations (radioimmunoassay) were performed after 24 hours, 1 week, and 4 weeks.Results: Bleaching agents increased collagen degradation, but C-terminal telopeptide of type I collagen (ICTP) values were higher when dentin was PA-demineralized. Nonvital bleaching plus PA promoted the highest collagenolytic activity, which was reduced after SB infiltration. Halogen light application did not influence ICTP values. At 24 hours, home bleaching exhibited high collagenolytic activity, which decreased up to 4 weeks. After 4 weeks of storage, all bleaching procedures showed similar values of collagen degradation, which were not different from those of PA-demineralized and resin-infiltrated dentin.Conclusions: All tested bleaching agents increase matrix metalloproteinases-mediated collagen degradation in dentin. This effect was not completely reverted after 4 weeks. Home bleaching induced the highest collagen degradation.
September 18th, 2011
Latest News Far and Wide
May 2013
News Archive

2013

May (58)
April (59)
March (66)
February (89)
January (103)

2012

December (60)
November (63)
October (64)
September (58)
August (93)
July (129)
June (126)
May (83)
April (81)
March (89)
February (79)
January (97)

2011

December (89)
November (78)
October (75)
September (65)
August (72)
July (117)
June (73)
May (90)
April (3)